Xiang Welding Industrial Co Ltd
AWS A5.1 / ASME SFA5.1 E7018-1
JIS Z3211 E4918
EN ISO 2560-A - E42 4 B 3 2
Notes on Usage
Welding Positions:
① Dry the electrodes at 350~400℃ (662~752℉) for 60 minutes before use.
② Keep the arc as short as possible, and avoid large width of weaving.
③ Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose to prevent blow hole at the arc starting.
Applications
AWS A5.1 / ASME SFA5.1 E7018-1 H4R can be used for welding of high tensile steel, such as bridges, buildings, rolling stock and low temperature used for steel structure.
Welding Position
Characteristics on Usage
AWS A5.1 / ASME SFA5.1 E7018-1 H4R is an iron powder low hydrogen type electrode. Its coating contains much iron powder,which increasing working efficiency. Its usability is good with direct current applications and verylow hydrogen electrode. (HDM < 5㎖/100g)
Current
AC or DC +